Wang Force-distance mechanical_property HiVacuum LiquidCell LFM Alkane Magnetostrictive Boron Polyvinylidene TemperatureControllerAFM #EC HardDiskMedia Ni-FeAlloy MultiferroicMaterials Bmp polymeric_arrays Blood IMT_Bucharest AdhesionForce optoelectronics Typhimurium LogAmplifier blended polymers Pvdf SurfaceOxidation CeramicCapacitor HydroGel Sapphire China Hafnia Nanopattern Defect ForceVolumeImage electrospinning
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
SRAM
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 3μm×3μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Sample Bias: 0.5V
- Scan Mode: CP-AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 3μm×3μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Sample Bias: 0.5V