ScanningSpreadingResistanceMicroscopy KPFM GaP self-assembled_monolayer Ni-FeAlloy TiO2 CancerCell Polypropylene LDPE MolecularSelfAssembly Film fluoroaalkane SolarCell single_layer cooling DNAProtein Copper solar_cell #Materials DiffractiveOpticalElements LightEmission PrCurve 3-hexylthiophene silicon_carbide Tungsten Calcite Bmp ForceVolume Ceramic LowDensityPolyethylene pulsed_laser_deposition Hexacontane ring shape Collagen CeNSE_IISc
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Carbon Nanotube on Si
Scanning Conditions
- System: XE7
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128