Copper Display non_contact FrictionalForce NCM Bio PVA IVSpectroscopy KevlarFiber Blood LogAmplifier Aggregated_molecules lithography 2dMaterials Resistance SICM Layer fluoroalkane Regensburg Hair SrO HDD SmalScan Worcester_Polytechnic_Institute organic_polymer Ceramic Inorganic_Compound Vortex GalliumPhosphide oxide_layer Growing hetero_structure IRDetector GranadaUniv ThermalDetectors
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BTO
Scanning Conditions
- System: XE7
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac