DIWafer FastScan Thermoplastic_polyurethane Change DataStorage silicon_carbide Display Conductivity SrO frequency_modulation CalciumHydroxide BTO SoftSample Subhajjit StrontiumTitanate PhaseImaging pulsed_laser_deposition Polyvinylidene LightEmiting food Graphene H-BN PhthalocyaninePraseodymium silicon_oxide TungstenThinFilmDeposition 2-vinylpyridine CrAu KelvinProbeForceMicroscopy LateralForce Wafer mechanical property Cross-section multi_layer mechanical_property Piranha
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic patterned array
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128