Self-assembledMonolayer NanoLithography Polyurethane MolecularSelfAssembly IIT-chennai Butterfly Polytetrafluoroethylene rubber PolyvinylAcetate temp PvdfFilm SAM ElectroDeposition Copper BFO PS_LDPE Domain MagneticPhase SetpointMode Ucl Fiber Sic Force-distance CBD Moire Gold kelvin probe force microscopy cannabis small_scan ThermalProperties Vacuum flakes temperature_control India Terrace
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen film phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan