PetruPoni Electrical&Electronics Solution HanyangUniv LiBattery Phenanthrene AlkaneFilm Sidewall Chloroform hetero_structure AdhesionEnergy Ananth Piranha FailureAnalysis single_layer Granada Logo graphene_hybrid MfmPhase cooling DentalProsthesis Bmp polyvinyl acetate PtfeFilter MagneticPhase LowDensityPolyethylene Au111 Pipette BreastCancerCell Steps IRDetector thermal_property CBD norganic silicon_oxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO Film Sputter Deposited onto Silicon
ITO-film, which was sputter deposited onto silicon. The grain size of those samples was influenced by changing the process settings in the Cluterline RAD sputter deposition system, one of the deposition tool platforms manufactured by Evatec.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.1Hz