Gallium_Arsenide IcelandSpar UTEM Polyimide Kevlar YttriaStabilizedZirconia CHRYSALIS_INC CP-AFM ForceVolumeImage SicMosfet TCS CuFoil Molybdenum_disulfide ChemicalCompound Perovskite NCM\ Aggregated_molecules cannabis CeramicCapacitor tip_bias_mode FM_SKPM Photovoltaics ConductingPolymer Defects DeoxyribonucleicAcid Thermoplastic_polyurethane 2dMaterials self_healing KAIST WWafer HighAcpectRatio FrictionalForce PtfeFilter AnodizedAluminumOxide HighResolution
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256