RedBloodCell Spain Film Nanofiber NtuEee LithiumNiobate Cobalt HardDisk NUS Iron IcelandSpar PS_PVAC CntFilm PhaseTransition MetalCompound ULCA IRDetector Nanotechnology Gallium_Arsenide Lift LDPE TCS Corrosion SelfAssembly LiquidImaging Photovoltaics DOE MagneticPhase Moire Annealed Display Fe_film Gallium SmallScan pulsed_laser_deposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System: NX20
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256