PetruPoni_Institute Perovskite HexagonalBN fe_nd_b pinpoint mode semifluorinated alkane Hysteresys Galfenol CntFilm Composite Beads Formamidinium_lead_iodide PhthalocyaninePraseodymium CuFoil Fluoride Sio2 Ananth Yeditepe Force-distance Steps PolyvinylAcetate CeNSE_IISc Croatia Molybdenum Polyaniline HafniumDioxide DLaTGS PhaseTransition Phenanthrene Ca10(PO4)6(OH)2 fluoroalkane TriGlycineSulphate pulsed_laser_deposition Bio BCZT
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe Thin Films
MFM images of Fe thin films (80 nm) epitaxied on GaAs(001) and then implanted with N-atoms. Images reveal weak stripe domains at magnetic remanence.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm