Galfenol Aluminum ito_film Conducting Foil Vac PinPointMode cannabinoid sputter SICM PtfeMembrane mechanical property Moire ForceVolumeImage GlassTemp cooling graphene_hybrid CBD LFM Strontium Piranha India Vortex Device Pinpoint PFM Pinpoint LowDensityPolyethylene ULCA PvdfFilm MembraneFilter PhaseChange BlockCopolymer temp BaTiO3 UnivOfMaryland
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferromagnetic Nanobars Array
Ferromagnetic nanobars arranged on a Penrose P2 tiling. The Permalloy (Ni81Fe19) nanobars are 810 nm and 500 nm long. The width and thickness of a nanobar amount to about 120 nm and 25 nm, respectively.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm