FrequencyModulation semifluorinated_alkane AIN Polytetrafluoroethylene Copolymer Writing semifluorinated alkane HexagonalBN PiezoelectricForceMicroscopy PtfeFilter Bio Liquid Tin sulfide epitaxy Gallium_Arsenide Dopped PhthalocyaninePraseodymium Biofilm PolyimideFilm Co/Cr/Pt Sio2 MagneticArray Friction Polyurethane temperature_control LiquidCrystal Terrace EvatecAG LithiumNiobate Celebration BloodCell Mechanical #EC AtomicSteps Neodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B Alloy
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm