HDD HydroGel Aggregated_molecules SiWafer Cobalt Leakage Memory Metal HighAcpectRatio MechanicalProperties LiIonBattery Bacterium Dimethicone Etch FrictionalForceMicroscopy Calcite StrontiumTitanate AtomicLayer Mosfet lithography AIN InorganicCompound Sphere MfmAmplitude Alkane VerticalPFM Chrome thermal_conductivity FM_KPFM CastIron Litho Magnetostrictive Bmp silicon_oxide Strontium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PVDF Fibrous Membrane
PVDF fibrous membrane made by electrospinning.
Scanning Conditions
- System: NX10
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256