Magnetic Indium_tin_oxide Optoelectronic WWafer CntFilm Sio2 HardDiskMedia Lanthanum_aluminate exfoliate Morphology Hair graphene_hybrid Chungnam_National_University Treatment Hafnia SAM Annealing CBD rubber PolyvinylAcetate BTO Battery TransitionMetal HighAspect Polydimethylsiloxane Transparent ShenYang Blood VerticalPFM Mechanical SrO CVD ScanningThermalMicroscopy PtfeMembrane CopperFoil
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512