EPFL TemperatureControlledAFM Permalloy AAO Polypropylene Nanofiber PhaseImaging mfm_amplitude CP-AFM Grain fluorocarbon 2-vinylpyridine Mfm Led InsulatorFilm Fujian Vanadate LogAmplifier self-assembled_monolayer Styrene LMF Polytetrafluoroethylene Kevlar solar_cell Sulfur fifber polyvinyl acetate SAM optoelectronics Corrosion Temperature GranadaUniv membrane biocompatible BoronNitride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polycrystalline ferroelectric BCZT
Scanning Conditions
- System: NX12
- Scan Mode: PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.4Hz
- Pixel: 256×256
- Sample bias sweep range for Piezoresponse curve: -10V ~ +10V