Current EFMAmplitude Patterns LiftMode Boron BreastCancerCell Lateral_Force_Microscopy China Tungsten_disulfide PANI FrictionForce AtomicSteps FM_SKPM CuFoil ScanningKelvinProbeMicroscopy IIT-chennai sputter HardDisk Hexylthiophene LiquidCell atomic_layer dielectric_trench PatternedSapphireSubstrat Friction Magnets Perovskite Yttria_stabilized_Zirconia Heating GaN Electical&Electronics AIN mechanical property Hexatriacontane TemperatureControllerAFM Mobile
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene
Scanning Conditions
- System: XE7
- Scan Mode: Conductive AFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256