PetruPoni_Institute SFAs Hydroxyapatite BlockCopolymer Dr.JurekSadowski flakes UTEM self_assembly ContactModeDots Sphere vertical_PFM ScanningIon-ConductanceMicroscopy Chloroform PolycrystallineFerroelectricBCZT PyroelectricDetector Display PVA FAFailureAnlaysis P3HT AdhesionEnergy Adhesive Metal Photovoltaics Ferrite Moire C36H74 Jason TempControl LiftMode Ferroelectric DeoxyribonucleicAcid fifber YszSubstrate Hysteresys MolecularSelfAssembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
P(VDF-TrFE-CFE)
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 0.5 Hz
- Scan Size : 2μm×2μm
- Pixel Size : 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)