dielectric_trench Co/Cr/Pt Ceramic piezoelectric force microscopy Vac Sphere electrospinning Battery align Foil ElectroChemical Tungsten_disulfide DIWafer Sic ConductingPolymer NUS_Physics #EC Tungsten Conduct Wafer Techcomp Led hydrocarbon Pinpoint PFM silicon_carbide MechanicalProperties LiIonBattery OrganicSemiconductor SingleCrystal AM_KPFM flakes INSP SrO Chloroform ForceVolumeImage
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semiconductor device, W-plug
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: ElectriMulti75-G (k=3N/m, f=75kHz)
- Scan Size: 2μm×1μm
- Scan Rate: 0.3Hz
- Pixel: 512×256
- Sample bias: +1V