Ceramics Piezoelectric dielectric trench HOPG Hole TyphimuriumBiofilm temp PANI FAFailureAnlaysis dielectric_trench Phthalocyanine Fluoride ScanningTunnelingMicroscopy Dental YttriaStabilizedZirconia BCZT Corrosion Blend flakes TransitionMetal PolyStylene AIN STO Spain PolyimideFilm HexagonalBN Co/Cr/Pt exfoliate AmplitudeModulation Mobile Hysteresys Polarization HBN Fet Wonseok
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Plate-shaped DNA origami
Scanning Conditions
- System : FX40
- Scan Mode: Tapping in Liquid
- Scan Rate : 1Hz
- Scan Size : 250nm×250nm
- Pixel Size : 512×256
- Cantilever : USC-F0.3-k0.3 (k=0.3N/m, f=300kHz)