EvatecAG exfoliate cannabinoid Chromium Bio contact P3HT CancerCell Nanostructure Ucl CaMnO3 atomic_steps mono_layer light_emitting mfm_amplitude Calcium Force-distance Au111 Mapping LightEmission Aluminium_Oxide Organic Polystyrene IVSpectroscopy Foil BariumTitanate HDD SiWafer Gong Hair CHRYSALIS_INC Optical CrystalGrowing Polyvinylidene_fluoride Plug
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen fibrils
Scanning Conditions
- System : NX10
- Scan Mode: Tapping in Liquid
- Scan Rate : ALL 0.3Hz
- Scan Size : 10μm2, 4μm2
- Pixel Size : ALL 256×256
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)