HexacontaneFilm C_AFM Hair CarbonNanotube HumanHair aluminum_nitride exfoliate NTU NiFe layers India CeramicCapacitor Pipette Ferrite Reduction MLCC Wildtype SiliconeOxide Polytetrafluoroethylene Co/Cr/Pt FrictionalForce DOE HOPG Cell Annealing University_of_Regensburg silicon_carbide Optical LightEmiting AtomicSteps FM_KPFM molecules Pattern Magnetic Chloroform
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Chip
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : All 1Hz
- Scan Size : 25μm×40μm, 15μm×40μm, 8μm×4μm
- Pixel Size : 2048×256, 2048×256, 1024×256
- Cantilever : OMCL-AC160TS(k=26N/m, f=300kHz)