Ananth Collagen Zagreb Fujian LateralForce HumanHair MolecularSelfAssembly Aggregated_molecules Non-ContactMode mfm_amplitude align Polyvinylidene SPMLabs Hexylthiophene NUSNNI HOPG hydrocarbon Cell TempControl LiquidCrystal Solution IcelandSpar PtfeMembrane BloodCell ring shape ContactMode Nanostructure TipBiasMode molecular_self_assembly Nanofiber Pore STO blended polymers EFM GlassTemp
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Mo film
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz, 0.8 Hz
- Scan Size : 5μm2, 15μm2
- Pixel Size : All 1024×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)