PANI FuelCell Spain Bismuth Lift Monisha Alloy KPFM blended polymers FAPbI3 OpticalElement TempControl CrossSection SThM PolymerBlend ForceVolume hard_disk_media Bmp nanobar SFAs self-assembled_monolayer 2-vinylpyridine Galfenol Electrode temperature_control membrane Solar Adhesive mono_layer Aluminum TemperatureControlledAFM phase_change Battery BariumTitanate Edwin
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Copper film
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : All 1Hz
- Scan Size : All 512μm×256μm
- Pixel Size : 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)