Vortex ferromagnetic PhaseTransition FrictionalForce Electrical&Electronics PyroelectricDetector STM plastics Hexylthiophene Layer single_layer molecule dielectric_trench Aluminum Celebration MoS2 Fiber fluoroalkane LightEmission Terrace SmallScan NusEce TemperatureControllerStage SAM SSRM electrospinning membrane Polystyrene Tin sulfide Metal DOE NTU Oxide Vinylpyridine Hafnium_dioxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semi-fluorinated alkanes
Scanning Conditions
- System : NX10
- Scan Mode: Sideband KPFM
- Scan Rate : 0.4 Hz
- Scan Size : 500nm×500nm
- Pixel Size : 256×256
- Cantilever : HQ: NSC14/CR-AU (k=5N/m, f=160kHz)