Granada BoronNitride Layer CarbonNanotube thermal_property 2d_materials SetpointMode SoftSample ContactModeDot LogAmplifier Pzt CancerCell Fiber Transparent Litho Memory Mosfet BFO Domain Metal LightEmission H-BN Insulator GaN Solar organic_polymer Inorganic Phthalocyanine VinylAlcohol Permalloy fifber block_copolymer CopperFoil TipBiasMode CrossSection
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
hBN-few layer Graphene
Scanning Conditions
- System : NX10
- Sample bias: 1.75 V
- Scan Mode: C-AFM
- Scan Rate : ALL 0.5Hz
- Scan Size : 200nm×200nm
- Pixel Size : 2048×2048
- Cantilever : AD-2.8-AS (k=2.8N/m, f=75kHz)