Layer MfmAmplitude Mobile Cobalt InsulatorFilm OpticalWaveguides Magnetostrictive silicon_carbide VerticalPFM ContactMode Floppy StrontiuTitanate DeflectionOptics C36H74 ImideMonomer bias_mode Typhimurium high_resolution HDD Lattice ChemicalCompound ContactModeDots ContactModeDot tip_bias_mode GranadaUniv FuelCell hard_disk_media Switching INSPParis Phase TappingMode Chemical Vapor Deposition Conducting DNAProtein MagneticForceMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Triple-cation perovskite
Scanning Conditions
- System : NX10
- Sample bias: 0 V, 0.5 V
- Scan Mode: C-AFM with PCM toolkit
- Scan Rate : 0.25 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 512×512
- Cantilever : ANSCM-PC (k=0.2N/m, f=12kHz)