Cell dielectric_trench Chrome Memory fluorocarbon semifluorinated alkane Force-distance PolymerBlend Bacteria Growth Protein Optic PyroelectricDetector Water HOPG SelfAssembly PolyvinylAcetate neodymium_magnets TemperatureControl mono_layer PDMS Polymer GranadaUniv molecules Lateral PS_PVAC Nickel Boron Moire Composition PVAP3HT Topography ChemicalCompound I-VSpectroscopy Wafer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Copper Foil
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.5Hz
- Pixel: 512512