Topography Cobalt-dopedIronOxide Scratch pulsed_laser_deposition Molybdenum_disulfide food FM_KPFM chemical_compound MLCC SelfAssembly PhthalocyaninePraseodymium FrictionalForce CeramicCapacitor AdhesionEnergy Bacteria PatternedSapphireSubstrat OpticalModulator AM-KPFM CompactDisk optoelectronics PolyvinylAcetate LiquidCell OrganicCompound suspended_graphene ContactMode WWafer INSPParis Tape TappingMode Boundary BreastCancerCell Epoxy FloppyDisk PolyimideFilm Semiconductor
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BFO (BiFeO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 5μm×5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512