margarine Wildtype Cell Magnetic Force Microscopy Photovoltaics BiasMode Nanostructure LMF LDPE single_layer MfmAmplitude nanobar semifluorinated_alkane Device Litho DiffractiveOpticalElements NtuEee ReflexLens LaAlO3 2d_materials Hafnium_dioxide mechanical property Ceramics Aluminium_Oxide PMNPT Imprint ForceMapping FrictionalForce Heat Solar Alloy Au111 HydroGel OpticalWaveguides Indium_tin_oxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Domain switching on PZT
Scanning Conditions
- System: NX10
- Scan Mode: Lithography, PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Litho. mode: Tip bias mode
- Litho. Tip bias: Black +10V, White -10V