INSPParis MeltingPoint Beads frequency_modulation NUSNNI #Materials HumanHair BloodCell Cell Platinum Ni81Fe19 Singapore PvdfBead BTO Co/Cr/Pt GalliumPhosphide MagneticForceMicroscopy Ecoli PrCurve Piezo EvatecAG Varistor ScanningSpreadingResistanceMicroscopy OrganicSemiconductor Growing dichalcogenide Adhesive VinylAlcohol Heating Reading CastIron AM-KPFM GaN PVAP3HT Sperm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcium Hydroxyapatite Crystal growing
HA crystal grows according to the annealing time. From 24hrs, the crystal becomes clearly.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256