Hexacontane Transparent AEAPDES Fujian fe_nd_b SAM Molybdenum polymeric_arrays ContactMode Celebration Ni-FeAlloy Laser Gallium Scanning_Thermal_Microscopy Polyvinylidene_fluoride Optoelectonics KPFM ScanningThermalMicroscopy University_of_Regensburg C60H122 hydrocarbon Fe_film Imprint Wang CuSubstrate neodymium_magnets MeltingPoint Materials HydroGel ReflexLens MolecularSelfAssembly SFAs Alkane Logo SKKU
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Imprint sample
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256