ConductiveAFM Styrene LateralForce ForceDistanceSpectroscopy PVA DomainSwitching Edwin Hysteresys LeakageCurrent cannabinoid sputter SiliconOxide StrontiumTitanate Global_Comm fluoroaalkane light_emitting PhthalocyaninePraseodymium Fujian FM_SKPM Vanadate LithiumNiobate Memory DOE MBE self-assembled_monolayer BloodCell CrAu ElectrostaticForceMicroscopy WPlug LiquidCell biocompatible ferromagnetic Potential 2d_materials Butterfly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PDMS liquid crystal
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512