Chromium Imprint Adhesion Non-ContactMode StyreneBeads Techcomp Ferroelectric Sphere sputter DataStorage GaP margarine SSRM Hair Ram Semiconductor Polyimide temperature controller AFM Phase food Platinum Au111 Fujian self_healing PolycrystallineFerroelectricBCZT SKPM Copolymer PinpointNanomechanicalMode Varistor heterojunctions CntFilm PvdfBead Strontium YttriaStabilizedZirconia Polyvinylidene_fluoride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ΙΙ
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256