LithiumNiobate Flake Imprint oxide_layer DataStorage ContactMode plastics AlkaneFilm Calcite PinPointMode Laser GalliumPhosphide PatternedSapphireSubstrat MLCC #EC Typhimurium LiquidCell HanyangUniv PhaseChange Oxide Indium_tin_oxide ForceVolumeMapping Adhesive Au111 thermoplastic_elastomers Titanate IISCBangalore SiliconeOxide BaTiO3 CalciumHydroxide ScanningSpreadingResistanceMicroscopy NTU Polyurethane optoelectronics hetero_structure
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BN thin film on Si
Scanning Conditions
- System: NX10
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256