Wildtype DNAProtein IIT-chennai Sperm Chrome LiquidImaging Bacterium PolymerPatterns CHRYSALIS_INC Ecoli Piezoelectric DIWafer SiliconCrystal FastScan Pore CaMnO3 FAPbI3 PVAP3HT CeramicCapacitor StyreneBeads Modulus VerticalPFM Nickel FAFailureAnlaysis Organic Heating Ni81Fe19 Lateral semifluorinated_alkanes Mosfet Zhi BiasMode Chungnam_National_University ForceVolumeMapping Metal-organicComplex
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen film phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan