Friction Device StrontiuTitanate hard_disk Polypropylene HafniumDioxide KevlarFiber hard_disk_media mfm_amplitude Fet Non-ContactMode Graphite Wafer ForceVolume BFO rubber MoirePattern WWafer cooling small_scan fifber Wildtype HumanHair UTEM TiO2 MagneticPhase Dimethicone InorganicCompound Hafnium_dioxide Mfm PolyimideFilm OpticalWaveguides KAIST Polarization Scanning_Thermal_Microscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Crystal
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: NCHR
- Scan Size: 2μm×2μm
- Scan Rate: 0.7Hz
- Pixel: 256 × 256
- Scan Mode: Non-contact
- Cantilever: NCHR
- Scan Size: 2μm×2μm
- Scan Rate: 0.7Hz
- Pixel: 256 × 256