University_of_Regensburg Fendb Piezoresponse piezoelectric force microscopy LaAlO3 CuFoil Cobalt LDPE LiquidCell GranadaUniv Metal Pzt Potential hard_disk_media heterojunctions pinpoint mode GlassTemp Ananth PetruPoni Electical&Electronics EFMAmplitude MetalCompound Crystal VinylAlcohol MembraneFilter SPMLabs Patterns CntFilm AM_SKPM Device Copolymer Zagreb Zhi DOE Filter
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36A Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 4μm×4μm
- Scan Rate: 0.3Hz
- Pixel: 512×256