Molybdenum Barium_titanate TemperatureControllerAFM Photovoltaics SolarCell Nanopattern optoelectronics Plug FastScan fifber Strontium Aluminum Oxide hydrocarbon India SICM Dental NUS Materials Ptfe PDMS fluoroaalkane LiftHeight Fujian Phthalocyanine Alloy PVAC Blood Cobalt PFM SiliconOxide TemperatureControl Austenite AAO IMT_Bucharest
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256