HOPG OxideLayer Heat Ca10(PO4)6(OH)2 biocompatible thermoplastic_elastomers CrystalGrowing Worcester_Polytechnic_Institute PtfeMembrane LeakageCurrent Calcite strontiu_titanate TemperatureControllerStage TungstenThinFilmDeposition PrCurve OpticalModulator Filter FAPbI3 HexacontaneFilm HiVacuum self_assembly Foil Korea F14H20 thermal_property GalliumPhosphide TemperatureControllerAFM MagneticPhase Polyaniline Resistance Reading CP-AFM Magnets MetalCompound Oxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cannabidiol(CBD) Molecules
CBD(concentration: 20 mg/mL) molecules assembled on Mica surface after solution rinsing Aggregated CBD molecules as a ring shape.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256