MechanicalProperty MoirePattern VinylAlcohol PFM Hysteresys BoronNitride LDPE PhthalocyaninePraseodymium piezoelectric force microscopy Litho OpticalWaveguides Domain Heat molecule Pyroelectric BloodCell Sadowski SurfaceOxidation Grain ScanningKelvinProbeMicroscopy TCS Step Sulfur FM-KPFM ScanningTunnelingMicroscopy PolyvinylAcetate Pinpoint PFM PatternedSapphireSubstrat Alkane India PolyvinylideneFluoride blended polymers flakes Nickel hydrocarbon
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 Layers on SiO2
A few layers of MoS2 on SiO2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256