AdhesionForce DNAProtein Polydimethylsiloxane IISCBangalore Wafer Graphite Hexatriacontane Silicon contact LiNbO3 Oxide HardDiskMedia Ca10(PO4)6(OH)2 CBD ShenYang PtfeMembrane Biofilm Scratch PFM Laser Memory SSRM Deposition molecule Vinylpyridine MembraneFilter Conductivity MeltingPoint CrossSection Inorganic_Compound margarine Dr.JurekSadowski Reading Wang SKPM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CVD Grown WS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256