Composition Iron Bacteria PUR WS2 Collagen ForceVolume Co/Cr/Pt VortexCore AtomicLayer SPMLabs Silicon HafniumDioxide PolyvinylAcetate membrane AAO MoS2 LightEmission TempControl Force-distance CalciumHydroxide neodymium_magnets Logo Conductance molecular_beam Phenanthrene PANI Vinylpyridine CarbonNanotube SRAM Beads HighResolution AM-KPFM Ni81Fe19 Reduction
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System: NX20
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256