VortexCore Hysteresys CompactDisk UTEM ChemicalCompound Oxide PolyStylene contact Wonseok ULCA Phase Metal-organicComplex Zhi VerticalPFM Hole Conductivity Tapping ContactModeDot Implant Bmp Fujian SurfaceOxidation Phosphide lithography phase_change temperature_control SurfaceChange Galfenol ForceVolumeMapping LightEmission bias_mode self-assembled_monolayer Magnetostrictive exfoliate Vortex
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Formamidinium Lead Iodide FAPbI3 Perovskite Film
FAPbI3 is an organic-inorganic hybrid perovskite material for nowadays high efficiency perovskite solar cell.
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256