Hafnium_dioxide Lanthanum_aluminate CVD molecules multi_layer Trench MLCC Fet LateralForceMicroscopy Imprint HOPG Fujian Adhesive fe_nd_b PhaseImaging Vac Thermal sputter Friction Roughness margarine StyreneBeads Logo Perovskite CeramicCapacitor biocompatible solar_cell Electrical&Electronics molecule Temperature BismuthVanadate hydrocarbon Stiffness Bacterium Polyvinylidene_fluoride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Composite Barium Titanate
PFM Quad color is overlaid on 3D surface morphology.
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256
- Scan Mode: PFM