Graphite Stiffness epitaxy Reading SingleCrystal ThermalDetectors CNT SrO Optoelectronic Growing Transparent Ecoli #EC HanyangUniv cannabinoid MBE GalliumPhosphide Bacterium light_emission ReflexLens OpticalElement Polyurethane HighAcpectRatio CVD HexagonalBoronNitride China suspended_graphene Foil molecular_beam organic_polymer Insulator Chemical_Vapor_Deposition Flake Perovskite temperature_control
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LPDE
Spincast layer of PS/LDPE blend on Si. Signal change by thermal conductivity difference.
Scanning Conditions
- System: NX10
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512