TemperatureControllerStage OrganicSemiconductor vertical_PFM Pinpoint PFM Subhajjit PhthalocyaninePraseodymium Iron LeakageCurrent BoronNitride MonoLayer Current graphene_hybrid LateralForce Plug Reading HardDisk margarine KevlarFiber piezoelectric force microscopy Magnets CrAu Mfm Insulator LiquidImaging UnivOfMaryland FrequencyModulation Vinylpyridine Chemical_Vapor_Deposition PetruPoni align Ceramics Device Yeditepe_University Mechanical Polypropylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Atomic steps on STO(110)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.62Hz
- Pixel: 512×512