Device HighAcpectRatio MagneticPhase PinPointMode ContactModeDots LiquidImaging Cobalt University_of_Regensburg Non-ContactMode ForceVolumeImage Graphene SmallScan DiffractiveOpticalElements Christmas KevlarFiber Ferroelectric Patterns MetalCompound Mosfet INSP Molybdenum_disulfide Ferrite BiVO4 ElectroDeposition align ItoGlass Holes UnivOfMaryland self_healing MultiLayerCeramicCapacitor Lattice PtfeFilter conductive Hexacontane LFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene
Scanning Conditions
- System: XE7
- Scan Mode: Conductive AFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256