PVAC MagneticPhase light_emitting IMT_Bucharest NUS_Physics Co/Cr/Pt Heating LightEmission Vanadate Terrace small_scan CarbonNanotube Fe_film FastScan MagneticArray Cell CntFilm PtfeMembrane LateralPFM Polyvinylidene FailureAnalysis HighAcpectRatio DeflectionOptics MultiLayerCeramicCapacitor SiliconeOxide Foil SmallScan Polyethylene biocompatible Layer Crystal Magnetic Force Microscopy NUSNNI ElectroDeposition cannabis
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
GaN on Si epi film
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : All 2 Hz
- Scan Size : 5µm2, 5µm2
- Pixel Size : ALL 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)