Piezo Hair Kevlar PANI 2dMaterials LogAmplifier light_emission SAM DiffractiveOpticalElements GaN Barium_titanate Cell SoftSample Pinpoint nanobar Foil BreastCancerCell Mapping Nanofiber CP-AFM HighResolution HafniumDioxide self_assembly TungstenDeposition IcelandSpar strontiu_titanate Polytetrafluoroethylene GalliumPhosphide UnivMaryland FM_KPFM C_AFM TyphimuriumBiofilm SicMosfet TiO2 Pore
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Escherichia coi (E. coli)
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 20μm×20μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)