ThermalProperties UnivMaryland PVAC food Film self_healing Vinylpyridine GaP Cell pulsed_laser_deposition Sulfur Ecoli OpticalWaveguides Domain hard_disk OxideLayer lift_mode SingleCrystal fluoroalkane CVD SPMLabs PyroelectricDetector Treatment FailureAnalysis NCM\ Gong Singapore Thermal heterojunctions Potential SSRM Barium_titanate TappingMode HACrystal Defect
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fractals of silver nanoparticles
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.31 Hz, 0.27 Hz
- Scan Size : 50μm2, 40μm2
- Pixel Size : All 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)