Workfunction MolecularSelfAssembly self-assembly amplitude_modulation Boundary Bio Hair LithiumNiobate BoronNitride TyphimuriumBiofilm molecular_beam Thermoplastic_polyurethane CeramicCapacitor Phase nanobar AnodizedAluminumOxide Laser LeakageCurrent IIT-chennai small_scan HBN Annealed dielectric trench temperature controller AFM layers OpticalWaveguide multi_layer Cell Friction Polyethylene UTEM ThermalConductivity PolyimideFilm Solution Semiconductor
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Copper Foil
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.5Hz
- Pixel: 512512